Problem innotec SNF 2004-08-01 14:03:02: Al (C2) source evaporated critically deep
aokyay at snf.stanford.edu
aokyay at snf.stanford.edu
Sun Aug 1 14:03:05 PDT 2004
Al source is significantly gone in the center. Also, the crucible is evaporated in the front and completely lost its circular shape... The Al source could now have undesired W incorporation.