Wet-etch of Ti

Ramesh Gopalan rameshgopalan at yahoo.com
Sun Jul 6 09:27:30 PDT 2008


Hello:
           I am trying to wet-etch off about 0.1-0.5um of Titanium deposited on Si substrate wafer - with Kapton (a polyimide, Teflon-like chemically resistant film) masking off areas that I dont want etched off.
    Any suggestions on which chemistry/ bench  I should use to etch Ti (I dont think the wbenches have the combination 10H2O:1H2O2:1H2SO4 - that is often suggested) - mix my own?
thanks for any suggestions,
Ramesh Gopalan