Request for metallization on PDMS and OE4100 on Metalica

Mahnaz Mansourpour mahnaz at
Wed Mar 17 11:16:57 PST 2004

Hi Claudia,

I do not see any issue with this as long as the PDMS has been cured.


Claudia Richter wrote:

> Dear Specmat Committee:
> We would like try a metallization process where we sputter either chromium or aluminum over cured PDMS or OE4100 on the metalica system. Would this be a process that we can do at SNF?
> Best regards,
> Claudia
> Claudia Richter
> Senior Staff Engineer
> Los Gatos Research Inc.
> 67 E. Evelyn Ave. Ste.3
> Mountain View, CA. 94040

More information about the specmat mailing list