Hi all --
What do you think? I take it that Pt is needed as a conductive layer
for FIB. It seems to me that if it is stripped and decontaminated as
per standard procedures (5:1:1 H2O:HCl:H2O2, followed by wbnonmetal,
followed by wbdiff clean) this should be OK for lampoly.