Koartan 6166 and 6125 silver pastes
Nathan Salowitz
Salowitz at stanford.edu
Mon Jan 31 17:39:41 PST 2011
Hello,
I would like permission to bring in Koartan 6166 and 6125 silver
pastes (MSDS attached).
Initial printing and drying to 125C will be performed at another
lab, therefore I would not be bringing in a liquid, but a dried form
already on wafers.
I would like to run them through their cure cycles in AW610_r at
600C and 900C respectively.
Please let me know,
Nate
-------------- next part --------------
A non-text attachment was scrubbed...
Name: MSDS Koartan 6125 2009.PDF
Type: application/pdf
Size: 31670 bytes
Desc: not available
URL: <http://snf.stanford.edu/pipermail/specmat/attachments/20110131/3a4d7076/attachment.pdf>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: MSDS Koartan 6166 2009.pdf
Type: application/pdf
Size: 25738 bytes
Desc: not available
URL: <http://snf.stanford.edu/pipermail/specmat/attachments/20110131/3a4d7076/attachment-0001.pdf>
More information about the specmat