Problem svgcoat SNF 2007-09-04 12:30:28: Spots at edges when using 3612
gsosa at snf.stanford.edu
gsosa at snf.stanford.edu
Tue Sep 4 15:49:23 PDT 2007
reduced the flow amount of the EBR with the micrometer adjustment. Too much flow causes the concentric EBR traces. Had to also modify the arm program to correct the timing between arm and dispense. May still need fine tuning. Also may need to move EBR valve closer to dispense head to improve the timing. GS