Problem wbmetal SNF 2010-10-20 17:46:24: resistivity takes a very long to reach 16 on the spin dryer
jhaydon at snf.stanford.edu
jhaydon at snf.stanford.edu
Tue Oct 26 08:58:45 PDT 2010
tested two times was able to achive 17.9 megohms both times. Problem is most likely wafer or casset.