Comment wbnonmetal SNF 2012-02-23 11:42:00: surface energy of my wafers was not normal

jwc at jwc at
Thu Feb 23 11:42:00 PST 2012

My wafers after coming off wbnonmetal had a hydrophobic state whicch is GOOD.  I manually stopped the SRD after a very long rinse cycle and noted my surface state was not correct. now hydrophillic.
moved to the other SRD to continue processing